Thermal Conductivities of [bmim][PF6], [hmim][PF6], and [omim][PF6] from 294 to 335 K at Pressures up to 20 MPa Tomida, D.; Kenmochi, S.; Tsukada, T.; Qiao, K.; Yokoyama, C.; International Journal of Thermophysics 2007, 28, 1147-1160
- Journal: International Journal of Thermophysics
- Sample Quantity(ies): Mass density
- Methodology: Constant-volume piezometry
- Phase(s): Liquid
- Substances:
Data
| T (K) | P (kPa) | ρ (kg m-3) |
| 294.1 | 100 | 1294.0 |
| 294.1 | 10000 | 1300.0 |
| 294.1 | 20000 | 1306.0 |
| 315.1 | 100 | 1278.0 |
| 315.1 | 10000 | 1284.0 |
| 315.1 | 20000 | 1290.0 |
| 335.2 | 100 | 1262.0 |
| 335.2 | 10000 | 1268.0 |
| 335.2 | 20000 | 1274.0 |
4997; 1-hexyl-3-methylimidazolium hexafluorophosphate; 00814