The measurement of thermal conductivity variation with temperature for Sn-20wt.% In based lead-free ternary solders íztürk, E.; Aksöz, S.; Kełlioćlu, K.; Marałlı, N.; Thermochimica Acta 2013, 554, 63-70
Data
wi = 0.2 g g-1, wi = 0.15 g g-1, P = 101 kPa
T (K) k (W m-1 K-1)
313 43.89
333 43.16
353 40.87
373 40.32
28366; tin + bismuth + indium; 01063:01897:04492